Click our video for more:
Increase your reliability,
not your customer
complaints.
©2017 Indium Corporation
Typical Voiding
>40% Void Area
Indium10.1
<10% Void Area
Indium8.9HF
<15% Void Area
Indium8.9HF
Solder Paste
Halogen-Free, No-Clean
Indium10.1
Solder Paste
Lowest Voiding Performance
No-Clean, Pb-Free
Visit us at: IPC APEX, Booth 1011
Contact our technical engineers today: techsupport@indium.com
Learn more: www.indium.com/avoidthevoid/SMTUS