80 SMT007 MAGAZINE I JULY 2021 Figure 10: Arrhenius plot of copper thin film corrosion rates in FoS chamber at 40°C and 15% relative humidity. Figure 11: Summary of corrosion rates of bare copper and silver serpentine thin films and thin films coated with acrylic or silicone. ALD-coated thin film corrosion rates are not included in these plots because their corrosion rates were within the limits of the experimental error.