APRIL 2018 I SMT007 MAGAZINE 53 Figure 14: Solder joints with most advanced crack growth after 3,000 cycles from cells 4-6. Pad type is noted parenthetically. Figure 13: Solder joints with most advanced crack growth after 3,000 cycles from cells 1-3. Pad type is noted parenthetically.